Answer
Dec 09, 2025 - 05:44 AM
When applying Accent Gold for Silver 24ct Paint 1gm, torch fire until the silver glows dull salmon and the gold accent appears bright orange; maintain this for 2 minutes. For kiln firing, place items on a kiln shelf and insert into a preheated kiln using gloves and tongs, as both the shelf and items will be very hot. Fire for 20 minutes at any temperature between 1110°F and 1650°F. Kiln tongs are recommended for safe and quick handling. This process ensures proper bonding and a beautiful gold accent when using Accent Gold for Silver.